Catalysts containing mixtures of NiO, MgO and ZrO2 were synthesized by the polymerization method. They were characterized by X-ray diffraction (XRD), physisorption of N-2 (BET), X-ray photoelectron spectroscopy (XPS) and X-ray absorption near-edge structure (XANES), and then tested in the partial oxidation of methane (POM) in the presence of air (2CH(4):1O(2)) at 750 degrees C for 6 h. Among the ternary oxides, the catalyst with 40 mol% MgO showed the highest conversion rates in the catalytic processes, but also the highest carbon deposition values (48 mmol h (1)). The greater the amount of NiO-MgO solid solution formed, the higher was the conversion rate of reactants (CH4), peaking at 40 mol% of MgO. Catalysts with lower Ni content on the surface achieved a high rate of CH4 conversion into synthesis gas (H-2 + CO). The formation of more NiO-MgO solid solution seemed to inhibit the deactivation of Ni degrees during reaction. The values of the H-2/CO product ratio were generally found to be slightly lower than stoichiometric. (C) 2012 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nickel oxide nonoparticles successfully synthesized by a polymer percursor method are studied in this work. The analysis of X-ray powder diffraction data provides a mean crystallite size of 22 +/- 2 nm which is in a good agreement with the mean size estimated from transmission electron microscopy images. Whereas the magnetization (M) vs. magnetic field (H) curve obtained at 5 K is consistent with a ferromagnetic component which coexists with an antiferromagnetic component, the presence of two peaks in the zero-field-cooled trace suggests the occurrence of two blocking process. The broad maximum at high temperature was associated with the thermal relaxation of uncompensated spins at the particle core and the low temperature peak was assigned to the freeze of surface spins clusters. Static and dynamic magnetic results suggest that the correlations of surface spins clusters show a spin-glass-like below T-g = 7.3 +/- 0.1 K with critical exponents zv = 9.7 +/- 0.5 and beta = 0.7 +/- 0.1, which are consistent with typical reported for spin-glass systems. (C) 2012 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The synthesis of zirconia-based ordered mesoporous structures for catalytic applications is a research area under development. These systems are also potential candidates as anodes in intermediate temperature solid oxide fuel cells (it-SOFC) due to an enhancement on their surface area [1-4]. The structural features of mesoporous zirconia-ceria materials in combination with oxygen storage/release capacity (OSC) are crucial for various catalytic reactions. The direct use of hydrocarbons as fuel for the SOFC (instead of pure H2), without the necessity of reforming and purification reactors can improve global efficiency of these systems [4]. The X-ray diffraction data showed that ZrO2-x%CeO2 samples with x>50 are formed by a larger fraction of the cubic phase (spatial group Fm3m), while for x<50 the major crystalline structure is the tetragonal phase (spatial group P42/nmc). The crystallite size of the cubic phase increases with increase in ceria content. The tetragonal crystallite size decreases when ceria content increases. After impregnation, the Rietveld analysis showed a NiO content around 60wt.% for all samples. The lattice parameters for the ZrO2 tetragonal phase are lower for higher ZrO2 contents, while for all samples the cubic NiO and CeO2 parameters do not present changes. The calculated densities are higher for higher ceria content, as expected. The crystallite size of NiO are similar (~20nm) for all samples and 55nm for the NiO standard. Nitrogen adsorption experiments revealed a broader particle size distribution for higher CeO2 content. The superficial area values were around 35m2/g for all samples, the average pore diameter and pore volumes were higher when increasing ceria content. After NiO impregnation the particle size distribution was the same for all samples, with two pore sizes, the first around 3nm and a broader peak around 10nm. The superficial area increased to approximately 45m2/g for all samples, and the pore volume was also higher after impregnation and increased when ceria content increased. These results point up that the impregnation of NiO improves the textural characteristics of the pristine material. The complementary TEM/EDS images present a homogeneous coating of NiO particles over the ZrO2-x%CeO2 support, showing that these samples are excellent for catalysis applications. [1] D. Y. Zhao, J. Feng, Q. Huo, N. Melosh, G. H. Fredrickson, B. F. Chmelka, G. D. Stucky, Science 279, 548-552 (1998). [2] C. Yu, Y. Yu, D. Zhao, Chem. Comm. 575-576 (2000). [3] A. Trovarelli, M. Boaro, E. Rocchini, C. de Leitenburg, G. Dolcetti, J. Alloys Compd. 323-324 (2001) 584-591. [4] S. Larrondo, M. A. Vidal, B. Irigoyen, A. F. Craievich, D. G. Lamas, I. O. Fábregas, et al. Catal. Today 107–108 (2005) 53-59.